Nanoindentation of Natural Materials
Hierarchical and Functionally Graded Microstructures
-
- CHF 270.00
-
- CHF 270.00
Beschreibung des Verlags
Nanoindentation of Natural Materials: Hierarchical and Functionally Graded Microstructures provides a systematic introduction and review of state-of-the-art statistical hierarchical and functionally graded structures found in bone, teeth, hair, and scales, from a nanoindentation perspective, including detailed microstructure and composition.
It covers the basics of hierarchical and functionally graded structures and nanoindentation techniques and detailed discussion with correlation micro/nano mechanical-structures
The book includes practical issues backed with experimental data