Die Casting Defects - Troubleshooting Guide
-
- £6.49
-
- £6.49
Publisher Description
A quick and easy-to-use guide intended for operator use on the shop floor. Contains casting photographs and photomicrographs for identification of 22 types of defects; provides brief descriptions and their causes; then guides the operator through a step-by-step series of process solutions to correct the defect.