Die Casting Defects - Troubleshooting Guide Die Casting Defects - Troubleshooting Guide

Die Casting Defects - Troubleshooting Guide

    • $129.00
    • $129.00

Descripción editorial

A quick and easy-to-use guide intended for operator use on the shop floor. Contains casting photographs and photomicrographs for identification of 22 types of defects; provides brief descriptions and their causes; then guides the operator through a step-by-step series of process solutions to correct the defect.

GÉNERO
Técnicos y profesionales
PUBLICADO
2003
20 de junio
IDIOMA
EN
Inglés
EXTENSIÓN
51
Páginas
EDITORIAL
North American Die Casting Association
VENDEDOR
North American Die Casting Association
TAMAÑO
1.3
MB